http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102898575-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_32a32316e15aaf21f987575aef40086d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F228-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F222-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F222-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-634 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-06 |
filingDate | 2012-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-05-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a41778b1ac3a0ea58879d84396bd17fb |
publicationDate | 2014-05-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102898575-B |
titleOfInvention | Ceramic slurry high-solid content promoter and preparation method thereof |
abstract | The invention relates to a ceramic slurry high-solid content promoter and a preparation method thereof. The preparation method comprises the following steps of 1, orderly adding water, a functional monomer and a part of an inorganic chain transfer agent into a mixer, mixing, and heating to a temperature of 70 to 80 DEG C with stirring to obtain a mixed solution I, 2, mixing an unsaturated carboxylic acid monomer, the functional monomer, the rest of the inorganic chain transfer agent and water into mixed monomers, and dissolving an initiator in water to obtain an initiator solution, 3, dropwisely adding the mixed monomers and the initiator solution into the mixed solution I in parallel, and after dropwise addition, carrying out heat preservation for 2 to 4 hours to obtain a mixed solution II, and 4, cooling the mixed solution II to a temperature of 40 to 50 DEG C, dropwisely adding a sodium hydroxide solution having a mass concentration of 30% into the mixed solution II until a PH value of the mixed solution II is in a range of 6 to 8, after dropwise addition, carrying out heat preservation for 0.5 to 1 hour, cooling, filtering and carrying out emptying to obtain the ceramic slurry high-solid content promoter. In a ceramic preparation technology, through utilization of the ceramic slurry high-solid content promoter obtained by the preparation method, ceramic blank strength and ball milling effects are improved. |
priorityDate | 2012-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 52.