http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102875709-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ddac65606de3b966e6f33acf1f1407c8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d7344f7b426556ad3a04cc689dc3b686 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-658 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-646 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-651 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-649 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-02 |
filingDate | 2011-07-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3e193ea39fb10a4ed47fbec8af80dc90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_98d820876d38ae91cfb0c5409384cf8d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0ce317653f7c65158caa0176922ae5ad http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_72d51579bbf591ac8f43d6766656b39c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_153a87e098d022366bf75ee27d18eceb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_64680be5520d901807c15db76ebec202 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_35785e599851e9fbc4dfcbe26ad844a3 |
publicationDate | 2014-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102875709-B |
titleOfInvention | Preparation method of catalyst component for ethylene polymerization reaction and catalyst thereof |
abstract | The invention relates to a preparation method of a catalyst component for ethylene polymerization or copolymerization and a catalyst thereof. The method comprises the steps of: (1) at a temperature of 50-90DEG, dissolving magnesium halide in a solvent system containing an organic epoxy compound and an organic phosphorus compound to form a uniform solution; adding an organic alcohol compound during or after the solution formation and leaving them to react for certain time so as to obtain a reaction solution; (2) in the presence of a boron compound and at a temperature of -30DEG C-0DEG C, subjecting the solution and a titanium compound to a contact reaction, or adding the boron compound after the contact reaction of the solution obtained in step (1) and the titanium compound, and raising the temperature of the mixture slowly to 50-120DEG C, leaving solids to precipitate gradually and form particles, after certain period of reaction, removing the unreacted material and the solvent, and conducting washing with an inert diluent so as to obtain a solid component; and (3) suspending the solid component in certain amount of the inert diluent, performing a contact reaction with an organic aluminium compound under a temperature of 0DEG C-50DEG C, and after certain reaction time, removing the inert diluent, thus obtaining the catalyst component. The catalyst provided in the invention has high catalytic activity and good hydrogen response. |