http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102872874-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4f0ad8476aa4a80345a4710c801c441a http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5ee516b21058331061801a0fcfa4b635 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10L3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-755 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-83 |
filingDate | 2012-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-01-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3e070dec171e77b1cd6c4a43e9713376 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9b7a82bbbcfb3792fc381e7fc45a99c9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c0e3cd34e3373ab129f15b477ed457f3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_da891e85bf8ea6de9e3da13d656b8dc7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_92f21b89827d050bfd306e2170f986f1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2a51c081de59d54e73a015d968d37a27 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f9db9113bab3bfd278300f1ed8a48780 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c673e8138c89761db682b73556f108a8 |
publicationDate | 2015-01-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102872874-B |
titleOfInvention | Loaded type nickel-based catalyst used for slurry bed methanation, and preparation method and application thereof |
abstract | The invention relates to a loaded type nickel-based catalyst used for slurry bed methanation, and a preparation method and an application thereof. The loaded type nickel-based catalyst is composed of, by weight, 10-40 wt% of NiO, 56-90 wt% of a carrier and 0-4 wt% of an auxiliary agent. The loaded type nickel-based catalyst is prepared by the steps of preparing a soluble salt solution of 0.5-1.3 g/mL nicdel nitrate and the auxiliary agent; adding a catalyst carrier and a soluble organic fuel to the salt solution in sequence; impregnating for 6-24 h while stirring; heating the solution for concentration in a water bath with a temperature of 60-90 DEG C after finishing the impregnation, or heating for igniting the solution at a temperature of 300-700 DEG C directly; collecting the combustion residue powder, grinding the powder and granulating, and reducing for 2-6 h with a reducing gas on a fixed bed at a temperature of 500-700 DEG C. The loaded type nickel-based catalyst has a slurry bed methanation process, and has the advantages of good and stable catalytic performance, and can be used for large-scale industrialization. |
priorityDate | 2012-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 64.