http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102816384-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_073b05644e3d35d6942a263a64bf6695 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2d07a0ffd1e2a9bed85094b97373aae9 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-14 |
filingDate | 2012-08-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-09-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_87844f49bf787a569435c08f7d3277da http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6c464a2537444a793286a75fa409de65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2751dd344ea207a5f6df4fe1cc9d7a2a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6dd98b23133b83d716633f57d8088e8e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6999fa22cc965f1d85e1f6617c9423cc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f039c5fa88a035225aca39b1c2873dc4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9f95ab61f1f4d119d232f5e34e4e022b |
publicationDate | 2014-09-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102816384-B |
titleOfInvention | Glass fiber-reinforced polypropylene material with shallow shrinkage mark and low warpage as well as preparation method and application thereof |
abstract | The invention discloses a glass fiber-reinforced polypropylene material with shallow shrinkage mark and low warpage as well as a preparation method and an application of the glass fiber-reinforced polypropylene material. The polypropylene material is prepared by using the following raw materials including 45-79% of polypropylene, 15-30% of chopped glass fiber, 1-20% of mineral fillers and 2-5% of grafted polypropylene, wherein the polypropylene includes high crystalline polypropylene as well as homopolymerized polypropylene and/or copolymerized polypropylene; the mineral fillers are one or more of barium sulfate, calcium carbonate or mica.The preparation method for preparing the glass fiber-reinforced polypropylene material provided by the invention uses the high crystalline polypropylene, the added chopped glass fiber and the mineral fillers for composite reinforcement and can effectively increase the cooling and curing rates of the material during the injection moulding process. The prepared product has the characteristics of shallow shrinkage mark, low warpage and high surface gloss, has the advantages of high flexural strength and modulus, good processability and low cost, can be used in household appliances and automotive industries, and can replace engineering plastic, and meet the requirements of high dimensional stability, high wrap and high mechanical properties of the parts. |