http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102807746-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c28bf379af69859baa280b299fd2693b |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-134 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-526 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-103 |
filingDate | 2012-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_103bb24c29902fc90cf10196036787fe http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2dc3ca84e8514504bce356eaf3343db7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_01f07b0341fc76401e102a0dd28c1d5c |
publicationDate | 2014-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102807746-B |
titleOfInvention | High-hardness and high-flowability PC/PMMA/AS (polycarbonate/polymethyl methacrylate/acrylonitrile-styrene copolymer) alloy and preparation method thereof |
abstract | The invention discloses a PC/PMMA/AS (polycarbonate/polymethyl methacrylate/acrylonitrile-styrene copolymer) alloy and a method thereof. The PC/PMMA/AS alloy with excellent mechanical properties, high hardness and high flowability is prepared. The PC/PMMA/AS alloy comprises the following raw materials in part by weight: 52-80 parts of polycarbonate, 10-20 parts of polymethyl methacrylate, 7-15 parts of acrylonitrile-styrene copolymer, 1-5 parts of ethylene-methyl acrylate copolymer, 1-5 parts of ethylene-methyl acrylate copolymer grafted glycidyl acrylate, 0.1-1 part of main antioxidant, 0.1-1 part of auxiliary antioxidant and 0.1-1 part of lubricating agent. The prepared PC/PMMA/AS alloy can be used for preparing communication equipment housings and electronic appliance product housings with higher requirements on surface hardness and surface luster. |
priorityDate | 2012-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links