http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102797031-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_daa5a466c918d96992db36ad5eb52436 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C30B7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C30B29-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G49-12 |
filingDate | 2012-08-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5a78c32d345f136f17a200cb34b6c88d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_49fd044bdff3966b58ce02d94a7d552f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dc054cc24b8d5c0c44c24c38065a428f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5e9f030841b2ce797bb87209debb30e9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_836bbfae0c0b73fdbbadabec62b66ab0 |
publicationDate | 2015-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102797031-B |
titleOfInvention | Preparation method of pyrite-type ferrous disulfide nanoscale single-crystal semiconductor material |
abstract | The invention relates to a preparation method of a pyrite-type ferrous disulfide nanoscale single-crystal semiconductor material. The preparation method comprises the following steps that 1, an iron source and trioctylphosphine oxide are mixed; and the mixture is dissolved in oleylamine, then is stirred and is filled with argon or nitrogen so that oxygen is removed and an iron source precursor is obtained; 2, the iron source precursor is heated in an oil bath with stirring so that an iron source solution is obtained; 3, a sulfur source is dissolved in oleylamine, then is stirred and is filled with argon or nitrogen so that oxygen is removed and a sulfur source solution is obtained; 4, the sulfur source solution is heated, then is extracted by a needle tubing and then is fast injected into the iron source solution; the oil bath for heating the iron source solution is heated; and the mixed solution undergoes a reaction to produce pyrite-type ferrous disulfide colloid; and 5, the pyrite-type ferrous disulfide colloid is cooled to a room temperature and then is added with a trichloromethane-ethanol mixed solution; the mixture is subjected to washing and centrifugation until an upper centrifugate is colorless; and the washed sample is sealed in a chloroform solution. The pyrite-type ferrous disulfide nanoscale single-crystal semiconductor material obtained by the preparation method has uniform particle sizes and morphology, and stable quality. The preparation method has good repeatability. |