http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102789842-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_215fd62f148bc5aab2bfc8e46ecd6126 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B13-00 |
filingDate | 2012-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b0e14566f6e322913f5a9278379b3950 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_13558553e58246b2ac820069a38f0e4f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_79e95552bec3e6a2ac01133235d6aa9b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d655225b011615a8f5e4a629bc8a5be1 |
publicationDate | 2014-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102789842-B |
titleOfInvention | Preparation method of conducting polymer/grapheme composite nanometer material |
abstract | The invention provides a preparation method of conducting polymer/grapheme composite nanometer material. The preparation method comprises the following steps that: (1) graphene is dipped in an oxidizing agent solution, and then is centrifugally separated and dried to obtain graphene which contains an oxidizing agent; (2) the graphene which contains the oxidizing agent and a conducting polymer monomer are respectively positioned in different positions in a closed container for reaction; and (3) the reaction product is centrifuged, washed and dried to obtain the conducting polymer/grapheme composite nanometer material. According to the preparation method disclosed by the invention, a solvent is not used, the condition is simple, the purity is high, and the structure of the graphene is not destroyed; film thickness is controllable, and the film thickness can be controlled by changing the proportion of the monomer and the graphene and the time of polymerization; the quality of the film is good, and the film thickness is uniform; the graphene and the conducting polymer have high compatibility due to the conjugate structure of the graphene and the conducting polymer; and the prepared composite material has high conductivity, excellent electrochemistry activity and good cycling stability, and can be applied in the fields of energy sources such as a super capacitor, a lithium battery and the like, and the fields of a sensor and the like. |