http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102725342-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2309-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2313-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2296 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2241 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-04 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61B42-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-22 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L13-02 |
filingDate | 2009-12-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2015-11-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-11-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102725342-B |
titleOfInvention | Do not use elastomer rubber and the rubber product of vulcanization accelerator and sulphur |
abstract | The invention discloses the composition that a kind of production comprises the elastomer thin film of carboxylated acrylonitrile butadiene latex, it does not use conventional sulphur and promotor sulfuration, thus reduces the possibility contacting health related problems that the speed caused by natural rubber latex proteins matter and the existence of promotor respectively sends out I type supersensitivity and tardy IV type supersensitivity.Also disclose and use latex composition to manufacture the dipping method of gloves as follows: make carboxylated acrylonitrile polybutadiene latex and methacrylic acid premix or alternatively use the latex through self-crosslinking, add zinc oxide, be adjusted to the pH level of 9-10 and dilute with water to obtain the total solids level of 18-30 % by weight; Gloves formed body is immersed in said composition to form the thin film layer of latex composition on formed body; Latex film on dry gloves formed body; Be cross-linked with the latex film made on gloves formed body. |