http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102674426-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0faf833dd70df2d6c8317bbafa707c6f http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ed82aaf3bc50098c6ecbbaac68aa8ecc |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2982 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01F11-188 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01F11-18 |
filingDate | 2012-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3fb42f99664bc1e7a222f1f56b62ec66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_377d9797ca436a6e591b841ff7a50d21 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_139008bd1e1de9ebe534932b0f99680c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6896c0f5c8e89cc1753ae437d637fa58 |
publicationDate | 2014-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102674426-B |
titleOfInvention | Preparation method of barium carbonate and product prepared by same |
abstract | The invention relates to a preparation method of barium carbonate and a barium carbonate product prepared by the same. The preparation method of the barium carbonate comprises the following steps: (1) adding barium hydroxide octahydrate crystals into an ice water bath, and mixing, wherein the temperature is controlled at 0-5 DEG C; (2) introducing carbon dioxide into the mixture obtained in the step (1) to react until the pH value of the reaction solution is 6.0-7.0; and (3) carrying out solid-liquid separation on the solid-liquid mixture obtained in the step (2), and drying the solid to obtain the large-specific-area high-purity barium carbonate product. The preparation method provided by the invention solves the problem of incompatible low strontium and large specific area in the existing preparation method, so that the barium carbonate product is no longer influenced by the sintering temperature, thereby enhancing the performance of the ceramic material. |
priorityDate | 2012-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 40.