http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102618237-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c860c0fe21a8ff1ca8f3234bf1f60628 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F290-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08B37-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K8-565 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-56 |
filingDate | 2012-03-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6434b78f35b5ed6449d08ff757e2edd0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7ded87b56c17aaba9dcc8518d7e7e7cd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9c7bf6c833779d4d824dac4a8bf1ed59 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a063202e48971e0b758fee1487b62d70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2bfc94e6cb9d4d0cf5c01e9753a6ea5a |
publicationDate | 2013-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102618237-B |
titleOfInvention | Polymer clay stabilizer containing Beta-cyclodextrin structure and synthesis method thereof |
abstract | The invention relates to a polymer clay stabilizer containing Beta-cyclodextrin structure and a synthesis method thereof, wherein the polymer clay stabilizer is used for restraining clay hydration swelling of an oil well. The technical scheme is as follows: the polymer clay stabilizer comprises the following materials and monomers in percentage by mass: 35-54.8% of acrylamide AM, 15-25% of sodium acrylate NaAA, 8-20% of 2-acryloyl-methyl-propyl sulfonate AMPS, and 0.2% of 2-O (propenyloxy-2-hydroxy-propyl)-Beta-cyclodextrin XBH; 0.02g of XBH and 2g of AMPS are added into a flask, and then 5.48g AM, 1.915g of AA and 0.585 g of NaOH are added into the flask, so a water solution with the monomer mass percentage concentration of 20% is prepared, and nitrogen is introduced into the water solution for 20 min; (NH4)2S2O8 solution and NaHSO3 solution are then added into the water solution while nitrogen is continuously introduced into the water solution for 10-20 min, and reaction is carried out at the temperature of 35 DEG C for 4-12 hours; and finally, the reacted solution is subjected to washing with absolute ethyl alcohol, smashing and drying to obtain AM/NaAA/AMPS/XBH quaternary polymer. The polymer clay stabilizer has good water solubility, viscosifying capacity, temperature resistance, salt resistance, anti-shearing capacity and clay-swelling restraining capacity, and reaches the swelling prevention rate of 84.37% towards sodium-montmorillonite. |
priorityDate | 2012-03-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 54.