http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102600869-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2e9ee764324721dc0acd562b9c583881 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J27-18 |
filingDate | 2012-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-02-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b827f67cfd9439963610400f448866e9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_524c9f35c665c03577e9bc4f8011df60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_559a47f4bcefe07010a9afe44ec633a4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_385e258243bfe985472ab9cb1570547f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f5de2f8725a41ae570ec26f89a4e9d60 |
publicationDate | 2014-02-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102600869-B |
titleOfInvention | Synthetic method of supported silver phosphate photocatalyst |
abstract | The invention discloses a synthetic method of a supported silver phosphate photocatalyst. The method comprises the following steps of: weighing 1-1.2mmol of silver nitrate, preparing into 10-15mmol/L of solution, and dropwise adding diluted ammonia water to obtain a silver ammonia solution; weighing 20g of bentonite, adding 80-100mL of distilled water, soaking for 10-12 hours to obtain a bentonite suspension, dropwise adding the silver ammonia solution into the bentonite suspension, continually stirring for 3-4 hours, ageing in a water bath of 80-85 DEG C for 24 hours, washing with water for 4-5 times, and adding 30-50mL of distilled water; and dropwise adding 0.01-0.1mol/L of phosphoric acid into an obtained product in the molar ratio of 1:3 of phosphoric acid to used silver nitrate, ageing in a water bath of 60-65 DEG C for 24 hours, washing with water repeatedly till a supernatant becomes neutral, and drying at the temperature of 105 DEG C to obtain the supported silver phosphate photocatalyst. The adsorption capabilities of the catalyst and a carrier are increased. |
priorityDate | 2012-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 38.