http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102586615-B

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0b75a05785dbfd86d27a87ddcdc5a524
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_586d4cf81b80890a2831249f930338b5
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P10-20
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B13-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B7-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B30-06
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B11-02
filingDate 2012-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date>
grantDate 2014-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a304a8fafe368e925da430c09f1a6a58
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_865a6a5aa68d830c56f8680d4fe84cf0
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d7ce9efab9e8eeaba173cd5ac2d95338
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2a1d6de2552bdb0e3afeb724b2740a66
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_92ff3a377ac351e8da356b3494fb9f0c
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0acfd7388d71defb2bf563490cdf25a7
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3c6d600b7632dafaa9a33bdedccc6266
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6d324a4b6ee75d4329f8290b734a1b2d
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d89531c6fea205e77a5865665996286a
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8261f82ac40568796122f4ca5507699a
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3829d98334ba2e9bf2d3e49e7ffa40ef
publicationDate 2014-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-102586615-B
titleOfInvention Method for efficiently enriching valued metals from complicated sulfur- and lead-containing waste residue
abstract The invention discloses a method for efficiently enriching valued metals from complicated sulfur- and lead-containing waste residue. The method comprises the following steps of: drying and grinding the sulfur- and lead-containing waste residue; adding coke powder and NaOH, smelting at the temperature of between 300 and 500DEG C for 30 to 60 minutes; and heating to the temperature of between 600 and 800DEG C, smelting for 60 to 180DEG C, and removing an upper dross layer to obtain a lower melt in which noble metals are enriched, wherein the recovery rate of lead in the melt is over 94 percent, the recovery rate of bismuth is over 96 percent, the recovery rate of gold is over 84 percent and the recovery rate of silver is over 95 percent. The method has the advantages of high recovery rates of metals, no environmental pollution, short flow and simple operation.
priorityDate 2012-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID23954
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID452706154
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419557109
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID16211716
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419577487
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID5359367
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID14819
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID14798
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID23985
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID428438116
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419593248
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID482532689
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID71586773
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID409060395

Total number of triples: 40.