http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102585574-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b1b95a0151fe6cf57f119866e3a10c11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cc3fbe5d3b08d24440b9e57be0201f53 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D4-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-00 |
filingDate | 2011-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-08-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_302b9d24ddd8edd37c83023ae1162475 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f7d108f0e7f428d7bb19e470304ca75 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_18e4b88fccd4b242ab8810f44b65e4ad http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_abf9137c12c0284a434209a6703ce414 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0123e4d3603991df94aa46c43fdd56c4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ae6eb3da049072d76a4ae6b054af4c3f |
publicationDate | 2014-08-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102585574-B |
titleOfInvention | Method for preparing ultraviolet (UV) curing flame-retardant coating material and UV curing flame-retardant coating material |
abstract | The invention discloses a method for preparing an ultraviolet (UV) curing flame-retardant coating material. The method comprises the following steps of: (1) preparing functional sol which is nano-sol modified by a silane coupling agent or sol generated by hydrolyzing alkoxide or the silane coupling agent; and (2) adding 20 to 70 mass percent of UV curing resin, 20 to 50 mass percent of reactive diluent, 5 to 40 mass percent of functional sol, 0 to 15 mass percent of nano antimony tin oxide slurry, 0 to 5 mass percent of glass microspheres, 3 to 5 mass percent of initiator and 0.1 to 6 mass percent of leveling agent into a dispersing kettle, and dispersing for 0.5 to 3 hours at the rotating speed of 1,000 to 2,000rpm to obtain the UV curing high-hardness wear-resistant flame-retardant coating material. The invention also discloses the UV curing flame-retardant coating material. The UV curing flame-retardant coating material can prevent heat transfer from the source, the surface temperature and internal environment temperature of the coating material are effectively reduced, and the aims of improving the working environment and reducing energy consumption are fulfilled. |