http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102585174-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ac31afbea1cbbb03498644721ffb4a62 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G61-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B32-184 |
filingDate | 2012-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a415b05ab6fe9ad29abc7651908fe79e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1f0346f649717acf006f2af8e82ed78b |
publicationDate | 2014-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102585174-B |
titleOfInvention | Method for preparing graphene/ poly (3,4-ethylenedioxythiophene) complex nano material |
abstract | The invention discloses a method for preparing a graphene/ poly (3,4-ethylenedioxythiophene) complex nano material. The method comprises the following steps of: taking an aqueous solution of a graphene oxide, adding 3,4-ethylenedioxythiophene monomers, and mechanically stirring for 30 minutes so that the aqueous solution and the monomers are fully mixed; removing redundant 3,4-ethylenedioxythiophene monomers through dialysis by using distilled water to obtain a graphene oxide/ 3,4-ethylenedioxythiophene complex; transferring 30 milliliters of the obtained solution to a microwave hydrothermal reaction tank, wherein the reaction temperature is 140 to 160 DEG C, the reaction time is 10 to 20 minutes, the power of microwave reaction is set to be 200 watts, and the reaction pressure is set to be 180 pounds per inch; and naturally cooling to room temperature, taking the sample out, filtering, and thus obtaining the graphene/ poly (3,4-ethylenedioxythiophene) complex nano material. Any oxidant or reducing agent is not required, and the reaction happens in the complex, so the method has the advantages of environment friendliness, convenience, fastness, good reproducibility and the like. |
priorityDate | 2012-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |