http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102583482-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d6a6f422b091ba12ea61d4adbf1b0e8e |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01F11-18 |
filingDate | 2012-02-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_51efb4a12f56c23c6588e82d4f88fb58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cf762c1edc8a8807b60f5a5cd8f54eae http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2ab8d77eedc8e4384b867c6ecebc6c19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c370933a43112a2f7c7971c7a2e4e8ee http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a129456eda80345f92575120d492bde0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_03ac625985a6f9a0ab38ae2916fdae9d |
publicationDate | 2014-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102583482-B |
titleOfInvention | Preparation method of flake-shaped aragonite calcium carbonate |
abstract | The invention discloses a preparation method of flake-shaped aragonite calcium carbonate. The preparation method comprises the following steps: (1) performing dry method coarse grinding to a shell raw material, soaking the shell raw material in lotion for 4-48h at normal temperature, utilizing roller watering to remove a cuticle layer and a prismatic layer, and obtaining nacreous layer calcium carbonate by washing; (2) adding water to the nacreous layer calcium carbonate, performing high-speed agitation to prepare slurry with the concentration to be 30-80wt%, adding a grinding aid with the weight being 0.5-5% that of the nacreous layer calcium carbonate, and using a stripping machine to perform wet grinding for 60-180min with zirconia ball, alumina balls or ceramic balls serving as grinding mediums; and (3) performing filter pressing and drying grinding to obtain the flake-shaped aragonite calcium carbonate. The preparation method of the flake-shaped aragonite calcium carbonate is simple in process and does not use a poisonous harmful reagent, the operation conditions are mild, the surface activity of the prepared flake-shaped aragonite calcium carbonate is good, and the flake-shaped aragonite calcium carbonate can be widely applied to industries such as plastics, papermaking, rubber, ink, coating, building materials, medicines and food. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105440140-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105440140-B |
priorityDate | 2012-02-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 51.