http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102532451-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a81e4e082850b58e5fad53705d23eeeb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-67 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C14C11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-102 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-10 |
filingDate | 2011-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-11-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8b137b3803ea06fc25ab4bf980d2942b |
publicationDate | 2013-11-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102532451-B |
titleOfInvention | Amine composition and application thereof, polyurethane resin and preparation method and application thereof |
abstract | The invention provides an amine composition which consists of diamine and monoamine in the molar ratio of (1.1-17.1):1. The invention further provides polyurethane resin and a preparation method thereof. The total amine value of the polyurethane resin is 1.20-20.0 mgKOH/g; the primary amine value is 8.7-38.8 percent of the total amine value; the secondary amine value is 5.6-82.6 of the total amine value; and the tertiary amine value is 8.7-55.6 percent of the total amine value. The preparation method comprises the following steps of: mixing high molecular dihydric alcohol with diisocyanate ester; adding a catalyst, and reacting at the temperature of 30-100 DEG C for 2-8 hours to obtain a dibasic alcohol polymer; reacting with a low molecular active hydrogen compound and a low molecular polyhydroxy compound; adding diamine which accounts for 0-70.6 percent of 100 percent by weight of diamine in the amine composition, and expanding a chain in an ester solvent; and adding the rest of diamine in the amine composition and all monoamine, and undergoing chain expansion and chain termination reactions in an ester and/or amine solvent to obtain polyurethane resin. The prepared polyurethane resin has the advantages of high physical and mechanical properties and high-temperature stewing resistance. |
priorityDate | 2010-12-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |