http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102532387-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_601e79cf39a0367e6a4afba407ed67d5 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F230-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D125-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F212-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-107 |
filingDate | 2012-01-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ccc866134bde72411766ef0106057b83 |
publicationDate | 2014-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102532387-B |
titleOfInvention | Solid acrylic resin and preparation method thereof |
abstract | The invention discloses solid acrylic resin and a preparation method of the solid acrylic resin. The solid acrylic resin comprises the following components by weight percent: 10-92 parts of metacrylic acid ester, 5-40 parts of acrylic ester, 0-40 parts of vinyl benzene, 0-30 parts of combination of acrylic acid and methacrylic acid, 0.6-2 parts of combination of azoic compound and hyperoxide, 1-10 parts of combination of N-dodecyl mercaptan, isooctyl 3-mercaptopropionate iomp and Alpha-methyl styrene dimer, and 0.2-2 parts of organosilicon monomer vinyltrimethoxysilane or gamma- trimethoxysilyl-propyl-methacrylate. The preparation method comprises the steps of a) prepolymerization: polymerizing the above components for 2-8 hours under 60-85 DEG C to obtain glycerol-state prepolymer; and b) oast polymerization: polymerizing the prepolymer with subsection temperature control in an oast, wherein the starting polymerization temperature is 50-120 DEG C, and the oast polymerization time is 20-40 hours. The solid acrylic resin and the preparation method of the resin have excellent adhesive force, heat resistance, water resistance, stain resistance and mechanical property. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107325217-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107325217-B |
priorityDate | 2012-01-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 57.