http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102532377-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ddac65606de3b966e6f33acf1f1407c8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d7344f7b426556ad3a04cc689dc3b686 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F136-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-42 |
filingDate | 2010-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1b9f45494ce36869ffcf9061b61c5930 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_55cd68e57c71cf9c36d6e4cd4bc55f3d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e17b5b8d049eb692fce77a170187f59 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a733ccb447cd239d3a52a685469fc3fa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1917fdcf49882bca13f98166aed8964e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f4a863a7a40d0e92be06eb4fbf7942c3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_71988ab236ab13360fa38260f726acf9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_998e496f375974af3a54d264857a2577 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_96dc8f0766196a5f960e933ea4f950f4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d382ac1ef0818f0c737999c7ff48cb62 |
publicationDate | 2014-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102532377-B |
titleOfInvention | Low cis-polybutadiene rubber as well as preparation method and application thereof |
abstract | The invention relates to a low cis-polybutadiene rubber as well as a preparation method and application thereof. The preparation method is characterized in that in a polymerization system formed by connecting at least two polymerization reaction kettles in series, in a non-polar solvent containing a structure regulating agent, an stable single-functionality initiator is adopted to initiate the polymerization of polybutadiene and then a conventional chain-end coupling technology is combined, so as to prepare the low cis-polybutadiene rubber having high Mooney viscosity and low SV (styrene viscosity) value (5% rubber-styrene solution viscosity at 25 DEG C). The properties of the prepared low cis-polybutadiene rubber are as follows: (1) the content of the vinyl group in a monomer unit is 8-14%wt; (2) a number-average molecular weight range is 80,000-110,000; (3) the Mooney viscosity ML[1+4] at the temperature of 100 DEG C is 45-65; (4) molecular weight distribution is 1.5-1.8; and (5) the SV value is 0.04-0.059Pa.s. The low cis-polybutadiene rubber synthesized by using the method can be applied to the field of plastic modification, and is especially suitable for preparation of a high-impact high-gloss grade polystyrene (PS) resin. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104558328-A |
priorityDate | 2010-12-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 149.