http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102344653-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b1776b91be1c4e0bfb6e4dfa95c96b91 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-183 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-00 |
filingDate | 2010-07-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-12-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a4aca5f9df8a1a5e7c47b59500567604 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ab6587bcb73a35b50097a5ccd19c084 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_edde68d263fbf04069ebabfcd039682f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_87b2bdbc644f0f1fcfe100dd7881af31 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a3d52c4da952a80cfbf0e5d5e137ebc3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0f47199e44b407602f890d3e1ae03da7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bac7c6f58620bca02dc4c223433ec4bb |
publicationDate | 2013-12-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102344653-B |
titleOfInvention | Polyethylene terephthalate (PET)/inorganic/organic nano-composite material and preparation method thereof |
abstract | The invention discloses a kind of polyethylene terephthalate/Inorganic/Organic Nanocomposites and preparation method thereof. Material is 48~94.905%: 0.095~12%: 5~40% composition of proportions by polyethylene terephthalate (PET), inorganic nano stick and three monomer block copolymers by weight percentage, wherein, be chemically bonded between PET and inorganic nano stick with Si-O-C, between three monomer block copolymer of PET and part withnn Chemical bonding,Surplus is scattered in PET; Method is that inorganic nano stick ultrasonic disperse is first obtained to dispersion liquid in glycol water,Again by dispersion liquid,Terephthalic acid (TPA) and ethylene glycol be placed in 220~250 DEG C,80~100min is stirred under 0.2~0.4MPa obtains mixture,Then,The oligomer of antimony acetate or zinc acetate and PET is first added into mixture,Place it in again 260~285 DEG C,90~150min is stirred under 10~50Pa obtains polymer,Later,First tercopolyureas kind monomer is three monomer block copolymers,It is blended with polymer melting again,Product obtained has high toughness and impact resistance. |