http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102159627-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-16 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-14 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-04 |
filingDate | 2009-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2014-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2014-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102159627-B |
titleOfInvention | Long-fiber-reinforced resin composition and molded article thereof |
abstract | Disclose is a long-fiber-reinforced resin composition comprising 50 to 90 wt% of a component (A) and 10 to 50 wt% of a component (B), wherein the component (A) contains reinforcing fibers at a content of 20 to 60 wt% relative to the total amount of the long-fiber-reinforced resin composition. [Component (A)] A long-fiber-reinforced thermoplastic resin pellet which comprises a thermoplastic resin, a modified polyolefin resin that has been modified with an unsaturated carboxylic acid or a derivative thereof, and reinforcing fibers, and which meets the following requirements (A-1) and (A-2): (A-1) the thermoplastic resin has a melt index of 100 to 250 g/10 min; and (A-2) the thermoplastic resin has a relaxation time (lambda) of 0.1 (sec) or shorter. [Component (B)] A polyolefin resin which meets the following requirements (B-1) and (B-2): (B-1) the polyolefin resin has a melt index of 20 to 70 g/10 min; and (B-2) the polyolefin resin has a relaxation time (lambda) of 0.23 (sec) or shorter. |