http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102046693-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c6b8e249edb72763b802986bcbf1f12f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-82 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-04 |
filingDate | 2009-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2013-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3be07aff94c9e79c4c1f9c7bb165545c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_75d51f046f2435a444fc6da70315621a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_282db81847812a0d2793a3ea13ee7943 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bdde6e5b5f2360c139f1c4039fb3e79a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_87933dd5fcb78d32e3bccf58b9af542c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8480dae9400886c4fd652717a842f268 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4f42af806db8041376ccc8cb8f0694eb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_01d01cc731e4ead9d76cf4a86d4bc2c6 |
publicationDate | 2013-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102046693-B |
titleOfInvention | Method for producing aliphatic polyester resin, and an aliphatic polyester resin composition |
abstract | Provided are an aliphatic polyester resin having a high molecular weight and, in the preferred state, a high melting point and excellent thermal stability and hue, and an effective method for the production of same. The method for producing the aliphatic polyester includes a melt polymerization process and a subsequent solid phase polymerization process, with a sulfonic-acid-group-containing compound as catalyst, and the amount of sulfonic-acid-group-containing compound added during the melt polymerization process, calculated as sulfur atoms, is from 300 to 3,000 ppm with respect to the raw material monomer, the sulfonic-acid-group-containing compound content after the solid phase polymerization, calculated as sulfur atoms, is from 300 to 3,000 ppm with respect to the product polymer, and more than 50% of the sulfonic-acid-group-containing compound remains after the solid phase polymerization. The aliphatic polyester resin composition contains in the aliphatic polyester resin an amount, calculated as sulfur atoms, of from 300 to 3,000 ppm with respect to the product polymer of a sulfonic-acid-group-containing compound having two or more sulfonic acid groups in one molecule. |
priorityDate | 2008-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |