Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c9999d359590090d93af9785ab9501e0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a87a44c3b46d4f3a7e41c7a4840d32a0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-298 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-157 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C30B5-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B33-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J19-00 |
filingDate |
2009-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2014-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_50ba8a675220637b4b9c183f6610beab http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_00a2997099d0a4545826952b48275c35 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_665b07209a3c6e33d2808e2f7c063667 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0bce4766e79d9635a87b84938eced5ae http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c12afbfc53e6e2dbfe0675e037f4f95e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5bc8b97005331ae3273b8f62a318cf69 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4d3cb59aaaf1cdbddd9c875ab86ed991 |
publicationDate |
2014-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-102036747-B |
titleOfInvention |
Process for producing colloidal crystal and colloidal crystal |
abstract |
Provided is a process for producing colloidal crystals from which a large single crystal reduced in lattice defects and unevenness can be easily produced at low cost without fail. The process for colloidal crystal production comprises: preparing a colloidal polycrystal dispersion in which colloidal crystals precipitate at a given temperature (preparation step); introducing into a vessel the colloidal polycrystal dispersion in the state of containing fine colloidal polycrystals precipitated (introduction step); and dissolving the colloidal polycrystals and then recrystallizing the dissolved polycrystals (recrystallization step). The crystals thus obtained have fewer lattice defects and less unevenness than the original polycrystals. |