http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102030933-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02T10-86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-548 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08C19-06 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-013 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-0016 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 |
filingDate | 2010-09-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2016-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-102030933-B |
titleOfInvention | Rubber composition for tire tread and pneumatic tire |
abstract | It is desirable to provide rubber composition for tire tread, wherein said rubber composition can stop reversion, and (outstanding resistance to rolling, reply petroleum resources are exhausted, pay close attention to CO can also to realize environmental performance in the way of well balanced 2 Discharge), wet earth-catching property, dry earth-catching property, control stability and durability (wearability, crack resistance) improvement. The present invention also aims to the pneumatic tire providing a kind of use for the rubber composition of its tyre surface. Described rubber composition for tire tread comprises: containing the rubber components of the 35 above epoxy natural rubbers of mass %; And white filler, wherein, total sulfur content is less than 1.75 mass %, and crosslink density is 7.0 × 10 -5 mol/cm 3 Above. |