Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1a55d1f45fc9fa78dc389b3d7d9a5fc2 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-5425 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J31-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-0091 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-57 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-08 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-57 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 |
filingDate |
2008-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2013-06-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ded560c6a645443112ba4cd2e0ded63b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_44ce62500a7428ae8ab7d32c5f9ce2bc |
publicationDate |
2013-06-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-101939367-B |
titleOfInvention |
Organopolysiloxane composition room temperature vulcanizable to elastomer and new organopolysiloxane polycondensation catalysts |
abstract |
The present invention relates to an organopolysiloxane composition which is vulcanizable from room temperature to an elastomer which crosslinks by polycondensation and contains no alkyltin-based catalysts, and also to new organopolysiloxane polycondensation catalysts. |