http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-101906187-B
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0cb011d981829bdcc85a40133a181da8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07F7-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07F5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F297-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F236-10 |
filingDate | 2010-07-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2012-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_00f0376839b9e0d72c6a91d71c563c2f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1f4d49b43104b52581b4215db3509113 |
publicationDate | 2012-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-101906187-B |
titleOfInvention | Application of rare earth compound with constrained geometry configuration in high-selectivity conjugated diolefin-styrene random or block copolymerization |
abstract | The invention discloses application of a rare earth compound with constrained geometry configuration in high-selectivity conjugated diolefin-styrene random or block copolymerization. The conjugated diolefin-styrene random copolymerization is catalyzed by using a catalysis system consisting of the rare earth compound with constrained geometry configuration, the conversion rate of the monomer is 94percent, the polymerization activity is 2.5*106g molLn-1h-1, the number-average molecular weight of the random copolymer is 0.01 to 1 million, the molecular weight distribution is 1.20 to 2.00, the styrene content of the random copolymer is 4 to 85 mol percent, and the cis-1,4 content of a conjugated polydiene segment is 90 percent. The conjugated diolefin-styrene block copolymerization is catalyzed by using the catalysis system, the conversion rate of the monomer is 100 percent, the polymerization activity is 1.5*108g molLn-1h-1, the number-average molecular weight of the block copolymer is 0.05 to 1.5 million, the molecular weight distribution is 1.20 to 1.50, the styrene content of the block copolymer is 5 to 91 mol percent, the syndiotacticity of a polystyrene segment is 100 percent, and the cis-1,4 content of the conjugated polydiene segment is 97 percent. |