http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-101636804-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8e0bf0928b608797b70bbc2b91c7e52e |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31504 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-0032 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-00 |
filingDate | 2008-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8761a3fd9be391810142244e7be8880d |
publicationDate | 2010-01-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-101636804-A |
titleOfInvention | Method for the production of a coating of a porous, electrically conductive carrier material with a dielectric |
abstract | The invention relates to the production of a coating of a porous, electrically conductive carrier material (1) with a dielectric (18), particularly for the use in a capacitor. The production method comprises the steps: infiltrating the carrier material (1) with a solution (2), comprising precursor compounds of the dielectric (18) and at least one solvent (12) and having a boiling temperature TS and a cross-linking temperature TN, drying the carrier material (1) infiltrated with the solution (2) at a drying temperature TT, which is lower than the boiling temperature TS and lower that the cross-linking temperature TN of the solution (2), until more than 75 wt.% of the solvent (12) is evaporated. |