http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-100480735-C
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d6a6f422b091ba12ea61d4adbf1b0e8e |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-04 |
filingDate | 2007-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2009-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d5e79783466e594f57bfb0087945b8cd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c174abc39869818cfe1c76a231774042 |
publicationDate | 2009-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-100480735-C |
titleOfInvention | Method for preparing organic silicon wear resistance coating of poly carbonate optical material surface |
abstract | A method for preparing organic silicon wear-proof coat layer of polycarbonate optical material includes coating substrate coating material on surface of polycarbonate optical material and drying it for 2-60 minutes at temperature of 20-100deg.c, coating intermediate coat material and drying it for 5-120 minutes at temperature of 20-100deg.c, coating wear-proof coating layer material and drying it for 30-300 minutes at temperature of 20-100deg.c for obtaining polycarbonate optical material with organic silicon wear-proof coated layer. |
priorityDate | 2007-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |