http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CH-576837-A5
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_573c805a24067a6ed13b959e1ef567ea |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K35-365 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K35-0272 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B23K35-3033 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K35-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K35-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K35-365 |
filingDate | 1971-12-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1976-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CH-576837-A5 |
titleOfInvention | Welding electrode - with a hollow metal core filled with powdered iron for welding cast iron |
abstract | A welding electrode comprising a hollow metal core filled with Fe powder, the core being an Ni base alloy is covered with a flux comprising =25 wt. % Ni powder, 4-18 wt. % Ni coated Mg, 18-47 wt. % alkali metal carbonates e.g. Ba, Ca or Sr, 6-18 wt. % deoxidants e.g. Fe alloys with Al, Si, Mn & Ti, =11 wt. % Fe powder, 2-13 wt. % Cu, 7 - 16 wt. % CaF2 or fluorspar, 4-24 wt. % carbon such as graphite, cellulose etc. and 1-6 wt. % kaolin. |