Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_72f6e20b6543452012b29ee7a6923f4f |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2251-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2258-025 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F27B15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F27B15-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D53-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B15-0013 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D53-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D53-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F27B15-09 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B1-02 |
filingDate |
2010-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2016-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1fb437d640545fc1debbb7da5d359ac1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_96887c50dac396227ca8eb6fe0b567a3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9b5bb83065ab03fc2b8822e82fd3d601 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cce740b158bcdb24355194cd542c9ffe |
publicationDate |
2016-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CA-2819207-C |
titleOfInvention |
Process and plant for treating ore concentrate particles containing valuable metal |
abstract |
The present invention concerns a process and a plant for treating ore concentrate particles containing valuable metal and having at least arsenic and sulfur containing components. The process comprises a two-stage roasting process comprising a first roasting step (1) made in a first roasting reactor (16) and a second roasting step (3) made in a second roasting reactor (17). A gas mixture is formed from the first process gas component (2) obtained from the first roasting step(1)and from the second process gas component (4) obtained from the second roasting step (3). Post combustion of the gas mixture is made in a post combustion chamber (6). The post combustion operates with said reducing and sulphide rich first process gas component (2) and the second process gas component (4) as oxidizer gas in order to decompose SO3 in the gas mixture to reduce the SO3 content. The risk of accretion formation and corrosion in the post combustion chamber and in subsequent steps is reduced. Finally the exit gas (7) is exposed to subsequent gas cooling and dust removal steps (8 to 11). |