http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-2770362-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8e8e7a2951d20a5667c05af5563390af |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L2400-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L2300-802 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L2300-404 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L2300-106 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L2300-102 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L2300-104 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L2300-202 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61F2-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L27-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L27-00 |
filingDate | 2009-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a3256e0e600d2502999cc861d34843e6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_78d2f20806b0ea78ed2baa465eec93a0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d78af002a3f68e8ccb7cf27f8debb205 |
publicationDate | 2011-03-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CA-2770362-A1 |
titleOfInvention | Medical supplies and method of producing the same |
abstract | Provided is a medical part with excellent antibiotic properties and antibiotic substantivity as well as high biocompatibility, and a manufacturing method therefor. After an anodic oxidation treatment, wherein a pulsed current with a frequency of 50 to 10,000 Hz is applied for an electrolytic treatment, is applied to a base material in an acidic electrolytic bath or an alkaline electrolytic bath so as to form a film, which has minute holes and/or minute protrusions and recesses preferably in the quantity of 5 x 104/mm2 or more on the surface of the base material, an iodine-impregnation treatment is applied so as to impregnate iodine or an iodine compound into said film. Polyvinyl pyrrolidone iodine, ß-cyclodextrin iodine, or silver iodine is desirable for the iodine compound. Furthermore, a biocompatible metallic material selected from Ti, Ti alloy, stainless steel, and Co-Cr alloy is desirable for the base material. The film may be formed by means of a chemical treatment, a thermal treatment, or a machining process, or a combination of these, instead of the anodic oxidation treatment. Thus, a medical part with excellent antibiotic properties and antibiotic substantivity as well as high biocompatibility can be manufactured easily and inexpensively. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102417741-A |
priorityDate | 2009-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 92.