http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-2762644-C
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_26c475bcbe0c24b485b6f37c45cd921f |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C2222-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-084 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-67 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C22-60 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-67 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C22-66 |
filingDate | 2009-11-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2017-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_51bffc043b5dce1f5b07aa47a8e23108 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7389142751e7c1856be6d215598f9e66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a2ef49f2a09d3144233dcedc5886eba1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_29e54d456415120737159045eb86525c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c012f341a885beeef0f885b3c9d682b6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3d5e8a2b9c71e34cfe715c588587a049 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ddabebd221019673f66da7dcb418ab95 |
publicationDate | 2017-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CA-2762644-C |
titleOfInvention | Mildly alkaline thin inorganic corrosion protective coating for metal substrates |
abstract | Disclosed is a neutral to alkaline inorganic conversion coating composition that can be applied directly to a metal surface without a phosphatizing pretreatment and that provides significant corrosion protection to the surface. The conversion coating composition preferably has a pH of from about 6 to 11 and more preferably from 8 to 10. In one embodiment, the coating composition includes at least one element from group IVB of the Periodic table, and optionally, at least one element from group VB of the Periodic Table, and an organic polymer. Preferably, the coating composition includes from 9 to 73% by weight, based on the total dry solids coating weights, of at least one element from group IVB of the Periodic Table. In another embodiment the conversion coating composition comprises at least one element from group IVB, a source of chrome, and an organic polymer. Preferably, the coating composition includes from 9 to 73% by weight, based on the total dry solids coating weight, of at least one element from group IVB of the Periodic Table. The conversion coating composition is a dry in place coating and produces a unique morphology upon drying of a continuous inorganic phase in which the organic polymer is dispersed as discrete polymer spheres. The coating composition is very versatile and can accommodate addition of a wide variety of organic polymers which can be added directly to the coating composition thus eliminating multistep coating processes. |
priorityDate | 2009-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |