http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-2610867-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8b9b07baa39efdd68eb1506a375245f8 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C5-3053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C229-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C7-413 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07F15-025 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C227-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07F15-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C229-16 |
filingDate | 2006-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b6becc140618d1089408ef3990eb861e |
publicationDate | 2006-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CA-2610867-A1 |
titleOfInvention | Ferric and acid complex |
abstract | A ferric and acid complex includes the reaction product of a chelant, iron oxide, a base, and a reaction promoter. The chelant has at least one carboxylic acid functionality. The reaction promoter has an Fe3+ ion. A process for preparing the ferric and acid complex in a vessel includes charging solvent, the chelant, the base, the iron oxide, and the reaction promoter into the vessel. The solvent, chelant, base, iron oxide, and reaction promoter are heated to a temperature of at least 170 ~F for a period of at least about 3 hours to form the ferric and acid complex. Due to the use of the reaction promoter having the Fe3+ ion, the process for preparing the ferric and acid complex results in reduced degradation of the chelant during processing and, thus, a high quality ferric and acid complex. |