http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-2506381-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d44399535bc2587a687971e4138a49b6 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-34 |
filingDate | 2005-05-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f560f9891a052faec760caec6484594c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7e5cccf6d4939570791bd8d931318e98 |
publicationDate | 2006-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CA-2506381-A1 |
titleOfInvention | Acrylic latex wood filler composition and method of making same |
abstract | In broadest terms, a wood filler composition of the present invention comprises: from about 11.50 to about 17.50 weight percent water; from about 14.40 to about 21.60 weight percent ceramic microspheres; from about 2.48 to about 3.72 weight percent wood flour; from about 0.32 to about 0.48 weight percent thickener; from about 0.80 to about 1.20 weight percent glass bubbles; from about 12.24 to about 18.36 weight percent acrylic latex emulsion; optionally from about 0.05 to about 0.20 weight percent of an adhesion promoter; and from about 36.06 to about 54.10 weight percent calcium carbonate. The composition preferably has a pH in the range of from about 8.4 to about 8.8. Further the composition preferably has a viscosity of between about 200,000 to 300,000 cps as measured on a BROOKFIELD RV viscometer (helipath on) with a TIE spindle at 20 rpm and 25 °C. |