Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be2258efa1dd0212d91e87b0487f4ede |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K8-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B26-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K8-46 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K8-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B26-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K8-44 |
filingDate |
2002-01-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4435f9b4edf76bbe94af25b551357d09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bddf8be3dc6a1002448d2dfc9fbf84f0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c02b54e2053816e289ff6547fd197415 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_549e3531115c37b28d01c51da09fe8cf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ee8521a270616d2dc11a6290e94c61d0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bf4cca304de26eaf7c3193def9a8211c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d9854a056ba9cf2a9f11177682ac8278 |
publicationDate |
2003-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CA-2460441-A1 |
titleOfInvention |
Methods and ultra-low density sealing compositions for sealing pipe in well bores |
abstract |
The present invention provides methods and ultra-low density sealing compositions for sealing pipe in well bores penetrating formations which readily fracture at low hydrostatic pressures. A method of the invention basically comprises the steps of providing a hardenable ultra-low density sealing composition comprised of an epoxide containing liquid, a hardening agent, a hardening accelerating agent, a light weight filler and hollow glass michrospheres having a density in the range of from about 5 to 8.5 pounds per gallon, placing the sealing-composition in the annulus between the pipe to be sealed and the walls of the well bore and allowing the sealing composition to harden therein. |