http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-2374135-C
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b637f9f45afd69585579aa44456b785c |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-0413 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-0263 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-0209 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F26B3-283 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F26B3-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-00 |
filingDate | 2000-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2005-07-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3b99545e4aa431ebb0aa1b05a80d37e0 |
publicationDate | 2005-07-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CA-2374135-C |
titleOfInvention | Multi-stage processes for coating substrates with liquid basecoat and powder topcoat |
abstract | Processes for coating metal or polymeric substrates are provided which include the steps of: (a) applying a liquid basecoating composition to a surface of the substrate; (b) exposing the basecoating composition to air having a temperature ranging from about 10°C to about 50 °C for a period of at least about 5 minutes to volatilize at least a portion of volatile material from the liquid basecoating composition, the velocity of the air at a surface of the basecoating composition being less than about 0.5 meters per second; (c) applying infrared radiation and hot air simultaneously to the basecoating composition for a period of at least about 2 minutes, the velocity of the air at the surface of the basecoating composition being less than about 4 meters per second, the temperature of the metal substrate being increased at a rate ranging from about 0.4 °C per second to about 1.2 °C per second to achieve a peak substrate temperature ranging from about 120 °C to about 165 °C, such that a dried basecoat is formed upon the surface of the substrate; and (d) applying a powder topcoating composition over the dried basecoat. |
priorityDate | 1999-05-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |