http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-2361309-C
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6fd83303735006e917a468db06a7a140 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4837 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-48 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K75-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C33-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C33-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 |
filingDate | 2000-02-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2009-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ad3adb67b01282860b6f56e6c9beffd7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_052864ac2c528d695305d3ce5690dda7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_77a5a1ddbf87afed0b3bd64703afe6c1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e56a44c28ab351bc42b41913c84a777f |
publicationDate | 2009-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CA-2361309-C |
titleOfInvention | Process for preparing moulded polyurethane material |
abstract | Process for preparing a polyurethane material in a mould in which process the following steps are conducted: 1. an external mould release agent is applied onto at least those surfaces of the mould which will be in contact with the ingredients used for preparing the polyurethane material and/or the finished polyurethane material; 2. the ingredients to be used for preparing the polyurethane material are fed into the mould; 3. the ingredients are allowed to react and to form the polyurethane material; 4. the polyurethane material so formed is removed from the mould and 5. steps 2,3 and 4 are repeated at least 10 times without repeating step 1, wherein at least 25% by weight of the ingredients used to make the polyurethane material, excluding water in this calculation when used, consist of polyether polyol having a functionality of 2-6, an equivalent weight of 500-5000 and an oxyethylene content of at least 50% by weight. |