Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9b0f615b92cd3bb66e8ea41483a2dc63 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6674 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4866 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 |
filingDate |
1997-07-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2006-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e772deeb77423ee3579f11f787307c90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ee137245dcb348ece3b2d28cf57e4af9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7f79f34dcba84f97fcc483daef5daf72 |
publicationDate |
2006-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CA-2258617-C |
titleOfInvention |
Polyurethane/urea heat-cured and moisture-cured elastomers with improved physical properties |
abstract |
Elastomers with improved physical properties, particularly hardness and rebound, may be prepared by the diamine chain extension or moisture cure of low isocynate group content, toluene diisocyanate-based prepolymers prepared from a polyol component comprising a high molecular weight, low unsaturation polyoxypropylene diol and a low molecular weight diol. The elastomers are useful for applications such as rollers and other applications where hardness and rebound are important. |