http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-2256707-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-651 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-6543 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F10-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-6465 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F110-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-654 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-651 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-646 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F110-06 |
filingDate | 1997-05-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a1c471e354b9949979ba9c85f2ea3bc5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_53182e7c5f398ffa42323eb3f0f18971 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eee53d72ba0c65a6bfd89f9df4255dce http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_93f48bc822f70d0d5c76b02bd911290d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b8f4ada2772da19aa0a21083d7fe287e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0983e5c51bfd99b6f75e5a4fa612039d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fd1b2098ac93106043fa1a9ddd1a26ab http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a02b69d03d04d0a8af06e4bf14244367 |
publicationDate | 1997-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CA-2256707-A1 |
titleOfInvention | Crystalline polypropylene, process for preparing the same, polypropylene composition, and thermoformed article |
abstract | The present invention presents crystalline polypropylenes that contain components insoluble in 64°C decane that satisfy the following characteristics (1) to (5) and are excellent in hardness and rigidity, high in melt tension, and excellent in molding properties, process for preparing such crystalline polypropylenes, and polypropylene compositions and thermoformed products that contain such crystalline polypropylenes. (1) The intrinsic viscosity (.eta.) (in 135°C decalin) is 0.5 to 10dl/g. (2) The molecular weight distribution (Mz/Mw) as determined by gel permeation chromatography (GPC; solvent: o-chlorobenzene, measurement temperature: 140°C) is 5 or more. (3) The pentad isotacticity (mmmm percentage), which is a stereoregularity index determined by the measurement of the 13C-NMR spectrum, is 98% or more. (4) The D value, determined using formula (1) below from the loss tangents, tan.deltaØ05 and tan.delta.10 measured at the frequencies, 0.05rad/sec and 10rad/sec respectively by a melt viscoelasticity measuring device under a temperature of 230°C and constant strain, and said loss tangent measurement frequencies, is 4.0 or more. (5) The molecular weight distribution (Mw/Mn) as determined by gel permeation chromatography (GPC; solvent: o-dichlorobenzene, measurement temperature: 140°C) is 6.0 to 20. It is preferable for the number-average molecular weight Mn of the components insoluble in 64°C decane to be 25000 or more. |
priorityDate | 1996-05-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |