http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-2220253-C
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1e70c0aeade92d7571d955d3b90ea06e |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2995-0087 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C70-24 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06N7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B3-26 |
filingDate | 1995-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2001-03-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b3fbd8bfd580d536f575585cb9fc75f9 |
publicationDate | 2001-03-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CA-2220253-C |
titleOfInvention | Abrasion-resistant composite sheet |
abstract | A composite sheet having a surface layer (17) of resin-impregnated pile-like vertical fibers (10) provides the sheet with unusually high resistance to abrasive wear. The surface layer (17) has a combination of characteristics that includes an effective pile-fiber concentration of 0.1 to 0.5 g/cm3, an over-all density of at least 0.4 g/cm3, a resin content of 25 to 90 weight % and a pile parameter of at least 0.3 grams/cm3. Preferably, the pile-like fibers (10) contained within the surface layer (17) are derived from particular contracted knit fabrics or contracted two-bar stitchbonded fabric s (20). |