Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ae598145c49ee7e4e46bdbbeb91e1f54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_804eba77ac505c35a04835b8b7a2b8ae |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31989 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K2240-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L33-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31906 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S428-921 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K3-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K3-15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L97-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B21-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K3-15 |
filingDate |
1994-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2002-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cd7fa258bc057d3f0bab8edba719c75f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7b5c88d9d6b8f97fa2aba36fa52737a3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f48e1dadf042277f203660eafda94d71 |
publicationDate |
2002-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CA-2164645-C |
titleOfInvention |
Hardened and fire retardant wood products |
abstract |
Wood products impregnated with from 30 to 80 % of a polymerizable monomer selected from the group consisting of hexanediol diacrylate and hexanediol dimethacrylate have excellent indent resistance. The wood products are impregnated with the monomer solution by placing the wood under a vacuum to remove air, contacting the wood with a monomer solution containing a polymerizable hexanediol diacrylate and/or hexanediol dimethacrylate monomer and from 0.5 to about 2 percent of a thermally activated free radical source as a polymerization initiator for a period sufficient to achieve the desired polymer loading. The wood is then heated under pressure to polymeric or cure the monomers. |