abstract |
This electrode uses a carbon fiber whose crystallites are 13 to 17 angstrom thick according to X-ray diffractometry. In a method for manufactoring the cell electrode using the carbon fiber, the carbon fiber is burned at a temperature between 900°C and 1,330°C. It is possible to provide a secondary cell having the characteristics of the carbon fiber and a high discharging capacitance. |