http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-2128409-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_05aa45bbbe92b502cb5976eadae82e24 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-4457 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-4492 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D13-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D163-00 |
filingDate | 1993-02-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4a9e7d533945d6f70d6a8523b9f36bb2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3e03f694d4a25fa213ce5e77559a4f3f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f68222572a8dd00c36f1aa2e2eb4a18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_41ca1af24a2a213400dc668b945f2ec7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_50192575499f0ef3d34dda8d605d65dc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ea7c44eb7ea8e021f13614cc9b78bdb3 |
publicationDate | 1993-08-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CA-2128409-A1 |
titleOfInvention | Method of coating electrically conductive, substrates, aqueous electrodip paints, process for the preparation of an aqueous dispersion of crosslinked polymer microparticles and dispersions prepared by this process |
abstract | The invention relates to a method of coating electrically conductive substrates using cathodically depositable electrodip paints. The invention is notable in that the electrodip paints employed contain crosslinked polymer microparticles which can be prepared by reacting (A) a compound which contains on average more than 1.0 epoxide groups per molecule, or a mixture of such compounds, and (B) a compound which contains not only a group reac-tive toward epoxide groups but also at least one ketimine or aldimine group in the molecule, or a mixture of such compounds to give a noncrosslinked intermediate product (C), which still contains on average at least one epoxide group per molecule, and dispersing this intermediate product in the presence of a Brönsted acid in an aqueous medium. |
priorityDate | 1992-02-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Predicate | Subject |
---|---|
isDiscussedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID425745069 http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID123139 |
Total number of triples: 22.