http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-2068808-C
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_eb626358cae4ac6ea406eebc4dce9b1e |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2351-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2327-06 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-02 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G101-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-10 |
filingDate | 1992-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2005-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9eb3e92e6e2be350478f26f440bd3488 |
publicationDate | 2005-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CA-2068808-C |
titleOfInvention | Process for producing a foamed polymer endowed with high resistance to solvents and high temperature resistance, and product obtained by means of said process |
abstract | A process for producing a foamed polymer comprises the steps of: mixing, in a dissolver, a mixture constituted by at least one isocyanate and a first unsaturated anhydride, which is charged to the dissolver in the liquid state and at a relatively high temperature; progressively cooling said mixture, with continued stirring, until a temperature not higher than 22°C is reached; adding to the mixture, with the latter being stilt kept with continuous stirring, a second aromatic anhydride, at least one foaming agent, a vinylidene compound, polyvinyl chloride) and a heat stabilizer; maintaining the mixture with continuous stirring, at said temperature, until a paste is obtained which is poured, after being preliminarily filtered, into a mould or container; curing said paste by charging the container to an oven at atmospheric pressure, and at a temperature not higher than 80°C; completing the curing of the paste-like mixture under pressure, by increasing temperature up to 180°C and subsequent cooling, until partially foamed germs are obtained; and completing the germ foaming process, by heating. |