Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fd9859f29d348e8f3fd06f6088b1177d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2495 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2350-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-8019 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4812 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-482 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-80 |
filingDate |
1991-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7b2839911c331c0aa1742a57f68566df http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d69913a08ba3768aa847f8e35fe65774 |
publicationDate |
1991-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CA-2035275-A1 |
titleOfInvention |
Polyurethane elastomers |
abstract |
Mo3346 IMPACT ABSORBING MEDIA ABSTRACT OF THE DISCLOSURE The present invention is directed to a solid polyurethane composition having a glass transition temperature of from -20°C to 0°C, having a Bayshore rebound of less than 20, and having a Shore A hardness of less than 80. Mo3346 |