http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-1320793-C
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a57e955216609e42b33abc9ba43decb2 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2110-0008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2375-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2110-0041 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-7607 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4072 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-36 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-36 |
filingDate | 1988-12-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1993-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e7b73bd3aa65d7e3493a17dd102f2453 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_43382f82acccaa7d54b6e51211da2a1f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a9b21b0bb75ecc52c8be36dbdcde59fa |
publicationDate | 1993-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CA-1320793-C |
titleOfInvention | Enhanced homogeneous polyurethane foam comfort cushioning and process for making same |
abstract | Abstract 1. Preparing a flexible polyurethane foam: a) placing a polyol polyurethane foam-forming reaction mixture in a reaction zone and allowing the mixture to rise thereby forming a partially cured cellular material b) applying a compressive force to the par-tially cured cellular material after the elapsing of a period of time after completion of the rise to thereby reduce the volume of the partially cured cellular material and c) removing the compressive force and completing the cure of the compressed cellular material. The cellular material has enhanced cushioning pro-perties including a unique and superior feeling of com-fort resulting from a soft touch yet with a deep firm support with an appropriate springiness to the foam. The polyol in the polyurethane foam-forming reaction mixture contains a mixture of d) from 90-10 parts by weight of a polymer polyol composition containing about 10-40% polymer solids and e) from 10-90 parts by weight of a base polyol having a molecular weight of at least 4500 up to 7000. The cellular material has a final volume which is reduced by about 10-60% of the original volume of the partially cured cellular material after the compressive force is removed based on the weight of the polyol com-ponents cellular material has a Support Factor of from about 2-5. |
priorityDate | 1988-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links