Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_706c81a1c8b030805deb4fb42cbd9a45 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-12 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-05 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J183-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J183-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-5425 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-05 |
filingDate |
1987-11-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1992-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_041c44842a5964a643633782b12fdeca |
publicationDate |
1992-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CA-1306559-C |
titleOfInvention |
Self-adhering polyorganosiloxane compositions |
abstract |
SELF-ADHERING POLYORGANOSILOXANE COMPOSITIONS ABSTRACT The combination of (1) a polyorganosiloxane composition curable by a platinum catalyzed hydrosilation reaction with (2) up to about 20 percent, based on the weight of (1), of a polyorganosiloxane composition comprising the mixture of a liquid hydroxyl-terminated polydiorganosiloxane and a moisture reactive organosilicon crosslinking agent, or the reaction product of said mixture, and an organotitanate catalyst yields elastomers that cure rapidly at temperatures of at least about 80°C. and cohesively bond to inorganic substrates such as glass and metal. The resultant cured elastomer exhibits a durometer of less than about 20 on the Shore A durometer scale. |