http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-1276054-C
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_07b3f7652bef102674d95b2457346b0a |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-246 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-24 |
filingDate | 1986-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1990-11-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_46846c085ee395da6b56f7d94cd936df http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bc870d9be40fd114be80e157afb5d67e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f66ab27ca4a46dd8e86e9ad0e70ddb02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eb56e7dc33db76d50b4730eb72d6f84a |
publicationDate | 1990-11-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CA-1276054-C |
titleOfInvention | Low temperature seal for anodized aluminum surfaces |
abstract | ABSTRACT This invention relates to a process for sealing an anodized aluminum surface by contacting the surface with an aqueous acidic sealing solution having dissolved therein zirconium and/or titanium and dissolved fluoride, said solution preferably including dissolved silicate and/or a dissolved thiourea compound, and including optionally a sealing auxiliary, the process being carried out at a temperature of no greater than about 40°C. |