Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_460c2d3884b7724541bf93de2a201dfd |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02T10-12 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F02M31-135 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05B3-141 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-4682 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01C7-025 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01C7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-468 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F02M31-135 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05B3-14 |
filingDate |
1985-12-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1990-08-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3717760de0c846fda6972df2e68cd400 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b326a61065e27f5cc46d4df1af572ac0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a5e486a460b12022a2072af9ca287bef http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c30dfbe1e7fa5a0464b892abffa7061a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6092703990f3e02162316c7302443530 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1b845c9cd094659a77c1ce7856471f6e |
publicationDate |
1990-08-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CA-1272589-A |
titleOfInvention |
Anti-reducing semiconducting porcelain having a positive temperature coefficient of resistance |
abstract |
ABSTRACT OF THE DISCLOSURE Anti-reducing semiconducting porcelain having a positive temperature coefficient of resistance comprises a barium titanate composition, and a flux containing 0.14 to 2.88 parts by weight of TiO2, 0.1 to 1.6 parts by weight of Al2O3 and 0.1 to 1.6 parts by weight of SiO2 per 100 parts by weight of the barium titanate composition. It has a high positive temperature coefficient of resistance which does not show any appreciable change in the presence of a reducing atmosphere, such as hydrogen gas or gasified gasoline. It need not be isolated from a reducing atmos-phere by a plastic or metallic enclosure, but can be exposed thereto. The flux may further contain a zinc, potassium or lithium compound. |