http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-1265895-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a4dd5b5181a9a9c1a1b5efc848c7606f |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-08 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-08 |
filingDate | 1985-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1990-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2a032cc768647ca2256c3d53789db4dd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ad4c437d71e065c76f92725b7852dab9 |
publicationDate | 1990-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CA-1265895-A |
titleOfInvention | Method of making plastics cellular material |
abstract | ABSTRACT This invention relates to a process for production of a plastics cellular material. The process comprises mixing a first mixture of a fast-curing resin that may be cured with an organic peroxide catalyst, a co-polymerizeable monomer, finely dispersed surfactants, finely dispersed gas releasing salt, hardening accelerators. The fast-curing resin and the co-polymerizeable monomer together in combination have a viscosity level in the range of 1875 CPS and 2725 CPS at 25°C. An acidic solution and organic peroxide catalysts are then mixed into the first mixture to form a second mixture that will foam in a controllable manner and cure to produce a foam material of desired density. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9463449-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012233184-A |
priorityDate | 1985-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 27.