http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CA-1259745-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F136-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F36-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08C19-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F136-06 |
filingDate | 1985-02-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1989-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_051624aa38cedd1356db8bf6ac50576f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_650c062bd75fcee0faed1d29c84de1a4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_04d1b99d6564709dd62d0ba392aff1f4 |
publicationDate | 1989-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CA-1259745-A |
titleOfInvention | Polybutadiene and process for preparing the same |
abstract | ABSTRACT OF THE DISCLOSURE A polybutadiene having an average 1,2-bond content of 18 to 32% by mole, a branched polymer chain content of 60% by weight or more and a Mooney viscosity at 100°C of 40 to 90, the viscosity of a 5% by weight concentration solution of this polybutadiene in styrene at 25°C being 60 to 90 cps, and a process for preparing the polybutadiene comprising starting the polymerization of 1,3-butadiene in an inert hydrocarbon solvent in the presence of a Lewis basic compound and an organolithium compound, the latter compound being in an amount of 0.5 to 3 millimoles per 100 g of 1,3-butadiene, at a temperature selected from the range of 30 to 80°C, carrying out the polymerization by controlling the temperature so that the temperature at the end of polymerization may be 5 to 40°C higher than the temperature at the start of polymerization, and adding to the resulting polymer solution a poly-functional halogen compound in an amount of 0.6 to 1 equivalent per equivalent of the organolithium compound to further react the polymer with the polyfunctional halogen compound. |
priorityDate | 1984-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links